Kinetics and Microstructural Control

· Growth by solid state diffusion of copper to the larger G-P zones (c) generates the θ''-phase of CuAl2 . The faces of these zones remain coherent with the matrix giving the maximum coherency strains.

From: Ashby & Jones, "Engineering Materials 2," Pergamon (1986)